HS Code |
673495 |
| Chemical Name | Titanium Boride |
| Chemical Formula | TiB2 |
| Cas Number | 12045-63-5 |
| Molecular Weight | 69.489 g/mol |
| Appearance | Gray to black powder |
| Melting Point | 3225 °C |
| Density | 4.5 g/cm³ |
| Purity | Typically ≥99% |
| Solubility | Insoluble in water |
| Thermal Conductivity | 60 W/m·K |
| Electrical Conductivity | Good electrical conductor |
| Mohs Hardness | 8.5-9 |
| Manufacturer | Sigma Aldrich/Merck/TCL Chemical |
As an accredited Titanium Boride (Powder) factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Titanium Boride (Powder) is supplied by Sigma Aldrich in a sealed, 100g amber plastic bottle with tamper-evident cap. |
| Shipping | Titanium Boride (Powder) from Sigma Aldrich/Merck/TCI Chemical is shipped in tightly sealed, inert containers to prevent moisture and contamination. The product is classified as non-hazardous for transport, but precautions against dust dispersion and exposure are observed. Packaging complies with international safety and transport regulations for laboratory chemicals. |
| Storage | Titanium Boride (Powder) from Sigma Aldrich/Merck/TCI Chemical should be stored in a tightly sealed container in a cool, dry, and well-ventilated area. Keep away from moisture, acids, and incompatible materials. Protect from physical damage and dust generation. Storage should comply with all local, regional, and national regulations for hazardous materials to ensure safety and stability. |
Competitive Titanium Boride (Powder) prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please call us at +8615371019725 or mail to sales7@bouling-chem.com.
We will respond to you as soon as possible.
Tel: +8615371019725
Email: sales7@bouling-chem.com
Flexible payment, competitive price, premium service - Inquire now!
In the chemical industry, every material tells a story through its properties and the way it is manufactured. Titanium boride powder stands as one of those advanced ceramic materials that have earned respect in workshops and laboratories. Over the years, our team has worked with TiB2 powder from raw material selection to finished product, honing particle size, purity, and morphology to meet the shifting requirements of the market.
Modern titanium boride powder doesn’t arrive by accident. Selection of high-purity titanium and boron sources matters from the outset, with chemical vapor deposition and self-propagating high-temperature synthesis (SHS) providing pathways to control crystal structure and limit impurities like oxygen and metallic inclusions. Routine monitoring during the synthesis process reveals just how sensitive TiB2 properties are to manufacturing conditions. I’ve learned this in the plant—minor temperature swings and variations in material ratios show up later in electrical conductivity and hardness. Our commitment to consistency has come from logging every batch, testing with X-ray diffraction for structure confirmation, and adapting the process until standard models deliver tight control over particle size and surface area.
Models we produce range from D50 of 0.3 microns for advanced coatings up to 5 microns for bulk composite components. We have prioritized purity above 99% for applications sensitive to foreign ion traces. The powder feels smooth and almost graphite-like due to controlled morphology, with angular and blocky grains tailored for improved green density. During my years at the mill, handling the finished powder, especially at the sub-micron level, feels like dealing with colloids. These finer grades tend to exhibit strong cohesion, requiring gentle deagglomeration techniques–a daily reminder that real-world powder needs careful handling, not just specification sheets.
Our TiB2 grades cover several appearances, from steel-gray fine powders to darker hues seen at smaller particle sizes. Material safety remains paramount; titanium boride is inert under normal processing temperatures and resists oxidation up to about 1000°C in air. We monitor for trace boron oxide formation, particularly after prolonged storage, opting for robust packaging to maintain long-term stability. I’ve personally witnessed old drums of unprotected TiB2 develop crusts that compromise downstream sintering—practical handling, storage, and moisture control matter as much as internal purity.
The difference between TiB2 powder and other advanced ceramics comes down to real-world performance. Sintered TiB2 offers a melting point over 2900°C, high flexural strength, and a Vickers hardness just over 25 GPa. The powder blends with aluminum to strengthen composites, where its presence in the matrix sharply increases wear and corrosion resistance. Unlike alumina or silicon carbide, TiB2 delivers excellent electrical conductivity even in compacted form, making it valuable for targets, crucibles, and cathodes in molten metal electrolysis.
Early on, customers were quick to ask how TiB2 matched tungsten carbide or hot-pressed boron carbide. The answer lies in oxidation resistance and mechanical stability. In aluminum reduction cells, the cathode blocks formed from TiB2 powder outperform carbon-based ones by offering both low wettability with molten aluminum and minimal erosion over long cycles. Lab results are good, but operators on actual potlines have come back with cathode blocks that maintain structural integrity far longer than those using traditional graphite.
Machinists who come from working with silicon nitride often ask about edge sharpness retention. Our experience shows that TiB2 inserts not only resist abrasive wear, but also dissipate static effectively, reducing tool chipping in high-speed dry cutting. Choosing which ceramic goes into the application depends on more than raw hardness–thermal shock resistance and wetting behavior often play a bigger part than the lab bench can reveal. TiB2 integrates well with oxide ceramics for hybrid composites, providing strength without sacrificing machinability.
Discussion around ‘specifications’ only makes sense when products enter actual workflows. Aerospace engineers tell us that TiB2-reinforced aluminum composites survive impact well and still shave precious weight from airframes. Powder metallurgy teams use our 2-micron grade to add toughness to tool steels, reporting longer die life in plastic molding lines. We’ve worked with researchers looking to produce cermet with TiB2 for turbine blade tips, exploiting both wear resistance and moderate toughness.
In the lab, high-frequency induction heating of TiB2 compacted parts produces nearly pore-free ceramics, thanks to sharp sintering behavior at temperatures between 1800–2200°C. We’ve supported sintering trials using both conventional furnace pressing and spark plasma sintering, where the fast heating rate and applied current produce dense, high-hardness bodies with grains at the sub-micron level. This sort of processing unlocks unique combinations of thermal conductivity and mechanical stability that few other ceramics offer.
Another design challenge appears in chemical equipment. Titanium boride powder delivers especially low solubility in hydrochloric and hydrofluoric acid, making TiB2 a suitable liner material for highly corrosive environments. Factories handling halide melts appreciate the material’s reluctance to react or dissolve, keeping process downtime to a minimum. We hear from operators that TiB2-lined trays, rods, and valves typically outlast competing materials by a margin that returns savings in maintenance and replacement parts.
High-performance powders come with manufacturing challenges. Uniform sintering downstream relies on careful deagglomeration and blending. I’ve dealt with batch-to-batch variation when suppliers of precursor metals altered purity levels. Small upticks in iron or nickel content sometimes show as brittle spots in finished components. We’ve built a practice of routine elemental analysis, using inductively coupled plasma (ICP) and glow discharge spectrometry to keep tabs on trace metallics. This watchdog work prevents later headaches and meets the demands of our most demanding applications.
Some customers ask why their compacts show pinholes or density gradients. From our side, achieving dense, crack-free sintered parts means starting with well-dispersed powder and using binder systems that burn out clean. Ball-milling provides a direct answer for most blend challenges, but over-milling tends to produce fines that promote dusting and breathing hazards. Years of experience taught us to adjust mixing speed and ball material depending on finished size. Die pressing at moderate pressures allows the powder to flow properly, filling cavities without bridging or layering. Our engineers always re-assess each pressing run, checking green body dimensions against finished parts to watch for unexpected springback.
Throughout manufacturing, titanium boride powder has carved its own niche. If you need the wear resistance of hot-pressed boron carbide, TiB2 will step in where electrical conductivity is also required. Compared to tungsten carbide, titanium boride’s density is much lower, making lightweight yet tough components for aerospace and automotive tasks more feasible.
Silicon carbide and nitride powders command a following in high-temperature bearings, yet they lack the same non-wettability to molten aluminum, limiting their use in smelting. In our first aluminum smelter job, we switched a customer’s cathode block from SiC to a custom TiB2 blend—the difference in block lifespan alone justified the move. The TiB2 block showed only minor surface wear after months in continuous use, while the previous SiC block suffered both corrosion and metal infiltration.
Electrical applications see similar differences. In electron beam vaporization and target fabrication, our powder's fine grain and high conductivity enable pure TiB2 or composite targets that ablate cleanly, supporting high-deposition-rate coating runs. Materials like AlN or ZrB2 might offer higher thermal conductivity or different reactivity, but TiB2 brings both conductivity and hardness in a single, cost-effective package. Customers in electronics and photonics report that devices fabricated using our powder keep contact resistance low, even under thermal cycling, where coatings from less robust ceramics rapidly degrade.
Markets shift as new requirements emerge. Recently, additive manufacturing teams have been experimenting with TiB2 powders in selective laser sintering. The high absorption of infrared wavelengths makes the powder behave differently than other ceramics, requiring new laser parameters during layer fusion. By collaborating with these users, we’ve adjusted our powder’s particle size distribution to suit flow and bed packing, listening to feedback about layer stacking and the clean cut-edge quality TiB2 can achieve.
Worker safety is always tied into production changes. Our shop employs glove boxes and dust collection, especially during fine powder handling. TiB2 is not classified as a hazardous dust, but all nanoparticulate materials present some risk during prolonged inhalation. After a handful of incidents early on, we overhauled our pouring and mixing stations to use negative pressure booths with HEPA filtration. Over time, operators have reported fewer skin and eye complaints, and airborne particulate count measurements dropped. Investing in robust safety infrastructure cuts downtime and attrition, ultimately improving morale on the floor.
Process water from wet-milling lines is filtered and recycled. Titanium and boron residues undergo collection and safe disposal: environmental audits look closely at both processing emissions and solid waste channels. By using closed loops, we keep both costs and environmental footprint manageable, answering the increasing regulatory focus on chemical waste. When newer regulations arrive, we’ve found that anticipating changes in process water and solid effluent standards makes transitions more cost-effective.
Materials science is not static; feedback from the field feeds directly into our product improvement cycles. One case that stands out: a propulsion device manufacturer reported early failure of coating life due to unexpected hydrothermal cycling. Running the same reaction in-house, we identified that tuning TiB2 grain size and surface chemistry improved adherence and doubled mean time to failure. In applications where cost is a concern, we often work with customers to mix TiB2 with reinforcing agents or tailorable oxide content to find an effective compromise between price and performance.
We see users ranging from advanced research labs conducting work in quantum electronics, to large-scale foundries seeking cathode production for aluminum electrolytic cells. Each of these segments calls for a different approach to powder compaction, sintering temperature, or composite blending. Our model range owes its breadth to direct requests: tight PSD control for plasma spraying, 99.5% purity grades for laser target manufacture, coarse grains for metal-matrix casting.
Simplified logistics means keeping a powder storage system near production lines. We make sure packaging resists both puncture and moisture, using reinforced multi-layer barriers. It takes less time to respond to user complaints when silos or drums are properly labeled and tracked by lot number—something we’ve learned after more than a few inventory mishaps. Rapid access to batch history often resolves customer issues well before they escalate.
Resource efficiency has shown up as a key trend in both technical work and regulatory expectations. We work to recover and recycle off-spec batches and by-products, sending spent powders through physical separation and re-milling to create new usable lots. This works especially well in coarse grades, where even tough, lumpy agglomerates can be broken down cleanly. Fine powder recycling is more delicate but necessary to avoid unnecessary landfill use. Every recovered gram counts in both bottom-line and environmental accountability.
Energy management also holds weight in today’s industrial climate. By fine-tuning furnace hold times, using digital feedback loops, and integrating waste heat recovery, we have found our sintering costs drop significantly. The leaner energy footprint boosts long-term competitiveness and lowers the carbon footprint per unit of powder. These changes have tangible impact—monthly bills go down, batch throughput goes up, reinforcing the value of operational transparency with our partners and end users.
No advanced ceramic stands still. Industries pushing for lighter, tougher, more corrosion-resistant components turn to materials like titanium boride powder to achieve those goals, and each successful deployment builds on real feedback, not just theory. We keep investing in R&D, staying close to academic research, and field-testing powder in new engineering environments. Direct dialogue with line engineers and machine operators remains the most honest way to track powder behavior, prompting us to keep refining our product at every stage—from raw synthesis to packaging.
Titanium boride powder changes the performance limits of aluminum, steel, and high-performance composites. As new composites come online and demands climb for wear and electrical resistance, the knowledge gained at the furnace, in the ball mill, and on the finished part continues to set the direction for the next generation of advanced powders. Our approach leans on the lessons earned through real production runs, material failures, and the creative solutions that arise when teams on both sides of the business share their experience honestly.